Steel Standard:EN 10025-3
Rolling Type:Structural steel plate,low alloy steel plate
Thickness:6mm-500mm
Width:1500mm-4200mm
Length:3000mm-18000mm
Heat Treatment:Normalised
Low temperature impacting test under -50 centigrade shall be done for structural steel plate S275NL.On longitudinal direction,the minimum values of impacting energy for S275NL test pieces shall be above 27 J,and on transverse direction,the minimum values of impacting energy for S275NL shall be above 16J according to steel standard EN 10025-3.Steel plate S275NL shall be supplied normalized or in an equivalent condition obtained by normalizing rolling.Xinsteel offer steel plate S275NL all over the world.
Technical Requirements & Additional Services:
♦ Low temperature impacting test
♦ Rolling under standard NACE MR-0175 (HIC+SSCC)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2
♦ Shot blasting and Painting,Cutting and welding as per end user’s demands
Mechnical property for S275NL Structural steel:
Thickness (mm) | ||||||||
S275NL | ≤ 16 | > 16 ≤ 40 | > 40 ≤ 63 | > 63 ≤ 80 | > 80 ≤ 100 | > 100 ≤ 150 | > 150 ≤ 200 | > 200 |
Yield strength (≥Mpa) | 275 | 265 | 255 | 245 | 235 | 225 | 215 | 205 |
≤ 100 | > 100 ≤ 200 | > 200 | ||||||
Tensile strength (Mpa) | 370-510 | 350-480 | 350-480 |
Main chemical elements composition of S275NL | ||||||
C | Si | Mn | P | S | Nb | V |
0.16 | 0.40 | 0.50-1.50 | 0.025 | 0.020 | 0.05 | 0.05 |
Al(total) | Ti | Cr | Ni | Mo | Cu | N |
≥0.02 | 0.05 | 0.30 | 0.30 | 0.10 | 0.55 | 0.015 |